TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Gumpert, Ben" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gumpert, Ben
Date:
Wed, 19 Nov 2008 13:13:52 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (79 lines)
Ioan,

But you can touch the component at 300°C max if you are using Pb-free?

Sounds like a process recommendation, not a real thermal restriction. I'd contact the vendor and discuss your process, it may be acceptable.

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Wednesday, November 19, 2008 11:50 AM
To: [log in to unmask]
Subject: [TN] Low temp solder alloy

Dear Technos,

 

I have another one for you.

 

We do these boards having 100 to 200 TH high power LEDs (5mm in
diameter) and see a fairly high return since after a few weeks in the
field some LEDs will die or become intermittent. So we sat down and
started reading the app notes, see an example at
http://www.cree.com/products/pdf/LED_Lamp_SolderingHandling.pdf

 

Well, it turns out that these components cannot be touched up with
solder irons at more than 280C, which is 530F. This is rather low and I
wonder if we are going to be able to get the solder up the hole.
Anyways, I am heading towards the shop, in order to do some testing.

 

In the mean time, I would like to have your opinion on low temp alloys I
could use for touch-up:

o        What alloy should I look at?

o        Can I use a low temp alloy to touch up eutectic SnPb joints?
Any compatibility / reliability issues related to the eventual mixture?

o        Any particular low temp alloy that is more compatible with
SnPb?

o        Anything else I should think about?

 

Thanks again,

 

Ioan


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2