     For those of you waiting for a part number (I promised a part number of the
     goldfinger covers we use) I ran into a tiny problem with the covers having
     been ordered ONCE years ago and now no one remembers who or where we got
     them from.

     But I am on a mission now, and will post the part number as soon as I get
     one.

     Regards,
     Jan Pelchat
     Sr QAE
     Benchmark Electronics
     Hudson Division


______________________________ Reply Separator _________________________________
Subject: [TN] Flux on Goldfinger
Author:  "Muhammad; Masdi" <[log in to unmask]> at 0UTG0ING
Date:    7/22/98 4:16 PM


        We are trying to reduce the number of units fail at system test due
to
flux on gold finger.  We know so far that the flux is deposited onto the
goldfinger during touch-up or rework and to reduce the contamination we are
planning to implement 'taping' the gold finger during touch up.  Need some
advice on what kind of tape we should use or is there any other simpler
solution
that we can implement.

Appreciate the help.

Masdi

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2