TECHNET Archives

October 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Date:
Fri, 28 Oct 2011 11:28:13 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Douglas Pauls <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (128 lines)
Ioan,
You have gotten a lot of good answers to the question so far and I will 
chip in my two cents worth.

Technically, there is no such thing as an RMA flux anymore, though the 
term continues in use.  RMA, Rosin Mildly Activated, was a flux 
terminology from the good old days of MIL-F-14256, the military flux 
specification.  It was cancelled in 1995 and directed people to J-STD-004, 
the current predominant flux specification in the industry.  The older 
rosin flux formulations that were termed RMAs, translated into ROL0, ROL1, 
or ROM0, depending on the flux and who you ask.  RMA fluxes are still 
available, though as the market shrinks for these, they are becoming more 
expensive, which encourages users to transition to something more modern.

Most people still using "RMA" flux are using the 15% solids, which is 
still pretty high, compared to low residue fluxes or water soluble fluxes. 
 Which means there is a significant amount of flux to clean off compared 
to other fluxes.

Isopropyl alcohol sucks as a cleaner, at least in my opinion.  People want 
to use it because it is cheap, available almost everywhere, does not 
impact industrial emissions much depending on where you are in the world, 
and is not  a health hazard, if you don't get too wrapped around the axle 
over flammability.  No way, no how would I ever want to clean an RMA flux 
with alcohol alone.  Does not work reliably.

In my experience, high solids rosin fluxes tend to be OK if you leave them 
alone, or if you totally remove them.  If you "kind of" remove them, you 
have a great deal of problems.  You remove the encapsulating effect of the 
rosin (which you want), but you free up the activators to cause havoc 
(which you don't want).  In my view, you want a really effective heated 
saponifier in an in-line aqueous cleaner, with a thorough heated deionized 
water rinse.

Doug Pauls



Ioan Tempea <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
10/28/2011 08:07 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea     <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Rookie question on RMA fluxes






Dear Technos,

 

Although I've been around in this trade of ours for quite a while now, I 
have never had the occasion to work with RMA fluxes. I need to know how 
this functions. How can RMA be cleaned, I've heard about alcohol...? Is 
regular aqueous wash enough? If alcohol only, do we need a special 
equipment? Anything else to know?

And, anyways, are RMA fluxes still available?

 

Also, I imagine most of you at ease with RMA have tried to talk your 
customers into converting to water soluble flux chemistries. How hard was 
that? Is it possible?

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]> 
W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2