TECHNET Archives

December 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 12 Dec 2007 16:20:19 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier /* <[log in to unmask]>
Parts/Attachments:
text/plain (25 lines)
Hi Mark,
A couple of issues—Question: how do you get storage temperatures of 110C 
unless you store on an enginine manifold or next to a furnace?
Actually, for your purposes the via fill material should have a CTE of 
roughly the same as the ED Cu—whant yopu need to be worried about is the via cap on 
top of which you want to build your micro-vias.

Werner



**************************************
See AOL's top rated recipes 
(http://food.aol.com/top-rated-recipes?NCID=aoltop00030000000004)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2