TECHNET Archives

December 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Date:
Wed, 19 Dec 2012 15:04:28 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
May be those small mill machines make temp stencil will do? You can use temp stencil material as your base material (I believe those are ESD save polymeric based. Can't remember where you can get them.  If I do, that would be old info. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Graham Collins [mailto:[log in to unmask]]
Sent: Wednesday, December 19, 2012 07:43 AM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] esd safe fixture materials

Good day TechNet!

We do high mix / low volume manufacturing, and often get oddball parts 
in packaging that is not conducive to pick and place machines (e.g. a 
bag of parts).  I would like to get a supply of material so that we can 
machine a tray to hold such parts and use it to feed them into the P&P 
machines.  We could make them out of material such as aluminum, but I'm 
thinking that the stuff commonly used for wave soldering pallets would 
be a lot easier to machine.  Can anyone advise a source for this material?

Thanks, and best wishes for the upcoming Christmas holidays!

-- 
regards,

Graham Collins
Senior Process Engineer
Sunsel Systems
(902) 444-7867 ext 211


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2