TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 24 Oct 2007 12:53:23 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (147 lines)
The information in that document contains very best practices that the
better board shops have been applying for years...I don't get how this is
being viewed and/or received as "new methods or requirements" for board
shops and assemblers???


I've read the Isola document, it does not contain anything new, it just
looks like someone (industry leader et al) finally wrote down what many
shops have been doing, and all shops should be doing...

I'm curious Ian, are you getting a stipend for pushing Isolas article? (this
was just a joke)

Franklin D Asbell

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna
Sent: Wednesday, October 24, 2007 8:13 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination of lead free PCBs

The Isola document referenced by Cheryl Tulkoff a few posts ago --
09-12-07 is a clue

http://www.isola-group.com/images/file/TechnicalBulletinleadfreeprocedur
es091207.pdf

I've heard talk of this from other laminate vendors but Isola has been
the first to bring this formally to the fabricators attention.

Ian




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Alexander
Sent: Wednesday, October 24, 2007 8:54 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination of lead free PCBs


Can you provide the document names that were published in August



Joel Alexander
Quality Assurance Manager
TT APSCO, INC. 




Ian Hanna <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
10/24/2007 08:47 AM

Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ian Hanna <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Delamination of lead free PCBs






These specific guidelines for lead-free were first published in august
of this year  -- this guidance is a departure from that given for modern
laminates, from roughly 1990 on up...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Franklin D Asbell
Sent: Wednesday, October 24, 2007 6:26 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination of lead free PCBs


(chuckle) A recent requirement!!! 

If your board supplier told you baking to remove moisture is a 'recent
requirement' then they are either very unknowledgeable about their
laminates or just plain deceiving you.

In either respect, good luck on being reimbursed.

Franklin D Asbell 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thomas, Ian (Ian) %
Sent: Wednesday, October 24, 2007 2:46 AM
To: [log in to unmask]
Subject: Re: [TN] Delamination of lead free PCBs

We just had a similar thing happen, with FR4 HR370.  Before we did'nt
bake prior to assembly as the boards came direct from the board house,
now we are seeing de-lam.  They told us that it is a recent requirement
that came from the material supplier that they forgot to inform us of.
Ours are 12 layer, stacked vias.  Currently we trying to get some money
back!

Ian Thomas

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2