TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w21D3-0007zbC; Tue, 4 Mar 97 14:53 CST
Encoding:
23 TEXT
Old-Return-Path:
Date:
Tue, 04 Mar 97 15:58:00 E
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10840
TO:
TechnetPost <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"LRCEE3.0.nJB.xk87p"@ipc>
Subject:
From:
"Lang, Michael" <[log in to unmask]>
From [log in to unmask] Wed Mar 5 15:
17:54 1997
X-Loop:
X-Mailer:
Microsoft Mail V3.0
Message-Id:
Parts/Attachments:
text/plain (35 lines)



Subject: Gold/Tin

     Darrell Daigle posted a request for info on the effect of solder on a
     gold-plated finger that is to be inserted in a gold socket.

     [Body deleted]

     Where the operating environment can lead to corrosion for any of these
     reasons, the corrective action is to remove the solder and replate the
     gold.


 ----------

I did not know it was possible to remove solder and replate gold...  There
has been a couple of emergency situations when we would have like to have
this capability, be it for PCB's or components, or other...  Can someone
provide specifics?


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2