Absolutely. A well-oiled factory works better :).
From: lduso - Diamond-MT.com [mailto:[log in to unmask]]
Sent: Monday, February 03, 2014 11:16 AM
To: TechNet E-Mail Forum; Stadem, Richard D.
Subject: Re: [TN] Wrist strap continuous monitoring
Oh yeah, lots of lotion. Especially in the winter.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com<http://www.Diamond-mt.com>
On Mon, Feb 3, 2014 at 12:09 PM, Stadem, Richard D. <[log in to unmask]<mailto:[log in to unmask]>> wrote:
We have been using CM systems for esd wrist straps and mat monitoring for at least 13 years. The only issue we had for constant alarms was if the operator failed due to dry skin. We have taught them to moisturize their wrist with approved skin cream such as R&R Moisturizing ESD Lotion, and that has pretty much fixed the issue. No other issues reported, the constant monitor system works much better than depending on daily wrist strap checks.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Kerr, Bryan (UK)
Sent: Monday, February 03, 2014 10:31 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] Wrist strap continuous monitoring
Hi Folks
Any consensus on the usefulness of continuous wrist strap monitoring ? I have been running a pilot line and have had a lot of problems due to constant alarms. Can't, at the moment, figure out if this is just a true reflection on variation in operator grounding or some failings in the monitoring system. Any experiences out there ?
Regards
Bryan Kerr
********************************************************************
This email and any attachments are confidential to the intended recipient and may also be privileged. If you are not the intended recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or distribute its contents to any other person.
********************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|