Dear Daan, When I use to check plated thru holes, I would look into the
barrels using self lit goose neck microscope, which can be put close to the
edge of the part and you can see under parts for a little distance , it
might be enough to see the condition of the mask thru the parylene under the
component. Hope it helps .Best, Jim Jablonsky
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Daan Terstegge
Sent: Monday, November 22, 2004 12:31 PM
To: [log in to unmask]
Subject: [TN] Solder resist inspection underneath components
Hi Technet,
I have a problem with a batch of boards of which I know that an
estimated 50% of them have a problem with the soldermask. The mask
(Dynamask 5040 dry film) is flaking off the board, and we didn't notice
this because the mask is only applied underneath the components (and all
of them have a low standoff, which makes it impossible to inspect).
Now we need to know which of the boards are affected, but desoldering
some of the parts to take a peek is not an attractive option as these
boards are already parylene coated.
I'm quite convinced that the answer is "no", but still I'd like to give
it a try and ask the following question:
Does there exists ANY technology (non-destructive) that makes it
possible to inspect the quality of the soldermask underneath components?
Best regards,
Daan Terstegge
PCB Assembly Department
Thales Land & Joint Systems
Tel +31(0)35 524 8297
Fax +31(0)35 524 8181
[log in to unmask]
Unclassified Email
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|