I have had this problem and have been able to recondition the holes using a
small drill bit the same size as the apertures (if they are round and not
oblong). Then use some very fine wet & dry paper on the stencil surface to
remove any small burs that may have been introduced.
We use Heraeus glue and have found a cleaning solution which copes very well
with this. Contact Adamtech (UK based) 44 (0)1785 286660
Mark
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.)
at 31/07/03 17:28
>Technet,
>
>We have been using IPA to clean SMT adhesive off the stencil during the
>build and ultrasonic wash after the build. Over time we started noticing
>residues of adhesive around the inside walls of the stencil appertures. The
>adhesive appeared to be cured and hardened and we tried many ways but were
>unsuccessful in removing it (brush with more aggressive solvent, ultrasonic
>clean etc.)
>
>We were informed that a specific proprietary cleaner solvent has to be used
>to clean the adhesive off the stencil effectively. The down side is a 5X
>cost compared to IPA and a 2-5 times slower evaporation rate.
>
>Does anyone have similar experience with cleaning SMT adhesive off the
>stencil? What is the common cleaning interval applied during adhesive
>printing? (we clean every 5 prints) Any suggestion in methods to
>recondition the stencil appertures?
>
>
>Rgds,
>Peter
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|