But if the tracks and the component terminations are solder, you won't
get a very reliable connection with silver loaded epoxy ....

Peter
--
--------------------------------------------------------
Peter Swanson        [log in to unmask]
INTERTRONICS            http://www.intertronics.co.uk

   INTERTRONICS is dedicated to providing quality
  material, consumable and equipment solutions to the
 electronics manufacturing and other technology based
  industries, with the highest levels of technical
           support and customer service.


-----Original Message-----
From: Joe V. Ottesen [mailto:[log in to unmask]]
Sent: 11 January 2001 7:09
To: [log in to unmask]
Subject: Re: [TN] RF Surface mount...


"Stephen R. Gregory" wrote:

> Hey all,
>
> We've got a job in here that's going to be a few RF assembies. It uses
> surface mount in the design, but the board doesn't have any soldermask
at all
> on the surface.
>
> The last time I dealt with something such as this, and tried to print
solder
> paste, place components, and reflow, all I wound-up with is a bunch of
> tomb-stones, and insufficient solder all over the board because the
solder
> wants to flow out all along the surface layer traces, and goes
where-ever it
> wants to go...because there's no soldermask to contain it.
>
> I'll try to post a picture of what I'm getting ready to deal with on
my
> free-drive tomorrow...
>
> This is not high volume at all, but from past experience it's my take
that we
> should just hand solder stuff like this...because we'll wind-up
touching-up
> everything anyway...have any of you ever dealt with stuff like this
before?
>
> -Steve Gregory-
>
>
------------------------------------------------------------------------
---------
> Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
>
------------------------------------------------------------------------
---------

Hey,

    Have you considered using conductive glue.....that stays were you
dispense it.


--

Joe V. Ottosen
Website      http://www.bbelectronics.dk

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2