TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 2 Feb 2009 08:12:55 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Sewell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Mike Sewell <[log in to unmask]>
Parts/Attachments:
text/plain (79 lines)
You might have your stencil house cut a "U" from copper foil - we use
Photoetch for our stencils and they list available material (including
copper) thickness in 2 through 10, 12, 15, 16, 20, 21, and 25 mil. You
could leave them in a sheet and cut them out as needed ...sorta like a
standard repair pad/trace frame.  

http://www.stencil.com/metals.html


Regards,
Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Monday, February 02, 2009 6:59 AM
To: [log in to unmask]
Subject: [TN] Jumper wire forming for fine pitch QFP?

Hello Technet
I've got a design where we have to run a jumper between two adjacent
legs of a fine pitch part.  So the jumper is a tiny piece of wire that
runs down the leg, across the foot, bends around in a U, and back up the
adjacent lead.  We hand form this, and the operators are not liking it.
I'm pondering getting the machine shop to try to make something we could
use to pre-form the wire for this, but it's a bit higher precision than
they usually work to.  The gap between component leads is about .012"

Does anything already exist in the tooling world to pre-form a wire in
this manner?  I don't want to re-invent the wheel if I can avoid it.


thanks,
 
Graham Collins
L-3 communications ES
Halifax Production Engineering



 



NOTICE OF CONFIDENTIALITY: This message and any attachments are solely
for the use of the individual or entity to which it is addressed and may
contain information that is privileged or confidential or controlled
technical data that is subject to the laws of Canada or the United
States.  If you are not the intended recipient, any disclosure, use or
distribution of the information contained herein is prohibited.  If you
have received this communication in error, please notify the sender by
reply e-mail and immediately delete this message and any attachments.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2