TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
multipart/alternative; boundary="----=_NextPart_000_0015_01C2F846.5000BCE0"
Sender:
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Date:
Tue, 1 Apr 2003 12:00:39 -0600
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Parts/Attachments:
text/plain (2115 bytes) , text/html (3411 bytes)
I'm curious...what specification calls out solderability testing to be performed at 'final inspection'???

Franklin


  ----- Original Message ----- 
  From: [log in to unmask] 
  To: [log in to unmask] 
  Sent: Tuesday, April 01, 2003 11:49 AM
  Subject: Re: [TN] Board Shop Audit


  To Susan and Franklin: 

  Just one more thought.  I have done this many times and at least 8 out of 10 will tell you that they do but only 2 out of 10 actually document the attribute.  Ask them if they do solderability testing in final inspection.  Most times you will not even find it on their finale inspection report. 

  Larry ---------------------------------------------------
  Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives
  Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
  -----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------


ATOM RSS1 RSS2