Anyone,

I have been told that a no clean paste post curing
will leave a white haze or residue around the well.
And, that this haze is a TIN OXIDE.  My question
is:  Is this ok?  Should we be concerned?  What 
chemistries could react with TnO2 causing corrosion?

My experience is oxide can be hazardous to the 
assembly, i.e. corrosion, tin wiskers etc.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2