You can use electroless nickel/palladium/gold for gold wire bonding. It is as good as electrolytic soft gold over electrolytic nickel.
roger
----- Original Message -----
From: Bresnan, Thomas
To: [log in to unmask]
Sent: Wednesday, September 18, 2002 2:05 PM
Subject: Re: [TN] gold wire bonding
Not sure how you'll accomplish this Steve.... Electroless nickel is applied to an etched pattern, thereby removing the electrical connections that you'd need for the gold electro-plating process. Unless you're "bussing" everything together, that is.
Tom
-----Original Message-----
From: Steve kelly [mailto:[log in to unmask]]
Sent: Tuesday, September 17, 2002 3:30 PM
To: [log in to unmask]
Subject: [TN] gold wire bonding
Gold wire bonding - we normally plate electroplated soft gold over electroplated nickel. Will electroplated soft gold plated on top of electroless nickel work as well. Thanks. Steve Kelly
PFC Flexible Circuits Limited
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
--------
|
|
|