TECHNET Archives

September 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Grossmann, Guenter" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Grossmann, Guenter
Date:
Wed, 23 Sep 2009 09:40:45 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (84 lines)
Hi Inge

Vibrations around? I just had recently a similar problem in an industrial environment. Failure analysis showed fretting on socket spring- contacts. When I made vibration measurements I found quite a spectrum of low level vibrations on the floor but a clear resonance at 28Hz in the rack.

Best regards

Guenter



>-----Ursprüngliche Nachricht-----
>Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Inge
>Gesendet: Dienstag, 22. September 2009 21:34
>An: [log in to unmask]
>Betreff: [TN] Knock, knock, knock on the heaven's door
>
>Well, not exactly that, but knock, knock, knock on a earthly board. One
>customer needs fix a intermittent problem asap. 19 inch racks with
>hundreds
>of PTH double sided boards, old technology, no BGAs, no QFMs etc, but
>lots,
>lots of DIPs. The edge contact fingers have a very thick and good gold
>over
>nickel, and the backplane connectors have really stiff double tongues.
>The
>contact pressure/sq is extremly high and I think the contact spots are
>really gastight once the board is plugged in. Now, they have electrical
>issues, and they've found, that the signals are interrupted or coming
>back
>when they knock on the boards. Someone is going to take a flight the
>other
>day to fix the problem. The electricians believe, stubborn as mules,
>that
>the only think needed, is to take out the boards and clean the edge
>contact
>fingers with a solvent and that will fix it. Myself, with quite many
>year's
>experience from connectors, I don't think that is the problem, because
>when
>such robust contact springs wipe along the contact fingers, they slide
>pretty deep into the gold and makes good connection. Each spring has
>double
>contact ridges, so the risk that some dirt should cause interrupts is
>minimal. There is more that talks against their theory, namely, that the
>problem is still there after plugging, deplugging more than once. I'm
>sure
>there is a solder joint issue, or maybe a bond wire problem in the
>packages.
>Logically, this later is more likely because you have thousands of
>solder/bond joints vs, just some one hundred edge connector ditto. A
>ratio
>like 10,000/100 per board. Without knowing all details, what is your
>general
>experience between the index finger and the big toe?
>
>/Inge
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2