I am using it to mount some chip packages and leds due to specific
requirement stated by customer.
I plan to use 7mils stencil?Somehow,will Ag epoxy with equal bonding
strength as solder after reflow?
thanks.sumxp
----- Original Message -----
From: "Lee parker" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Sunday, February 26, 2006 12:23 AM
Subject: Re: [TN] Printing Ag epoxy
> What is the application?
>
> If you are trying
> Smxp
>
> What is the application?
>
> If you are trying to fill vias this is normally done after forming only
the holes to be filled and consequently a stencil is unnecessary and would
increase the aspect ratio of the hole to be filled.
>
> Best regards
>
> Lee
>
> J. Lee Parker, Ph.D.
> JLP Consultants LLC
> 804 779 3389
>
>
>
> ----- Original Message -----
> From: sumxp<mailto:[log in to unmask]>
> To: [log in to unmask]<mailto:[log in to unmask]>
> Sent: Saturday, February 25, 2006 4:53 AM
> Subject: [TN] Printing Ag epoxy
>
>
> Hi,
>
> Anyone had experiance in using solder paste printer to print Ag epoxy on
> pcb?Is it doable?What is the right viscosity on Ag to perform Ag
printing
> process?
>
> Thanks.sumxp
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]> with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:Listserv@ipcorg>: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentp
age.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori
at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>
>
> --
> Internal Virus Database is out-of-date.
> Checked by AVG Free Edition.
> Version: 7.1.375 / Virus Database: 267.15.11/264 - Release Date: 2/17/2006
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|