TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
annie laberge <[log in to unmask]>
Date:
Mon, 28 Apr 1997 09:16:23 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (108 lines)
Hello Technet...I have a question regarding this discussion:

How can I know if a soldermask is compatible with a flux ? Do the suppliers
of mask / flux have this information ? Or we probably need to do some
tests...What kind of test ?

Thank you in advance



>Resent-Date: Thu, 24 Apr 1997 17:58:30 -0700
>Resent-Sender: [log in to unmask]
>Old-Return-Path: <[log in to unmask]>
>Date: Thu, 24 Apr 97 17:12:46 cst
>From: "ddhillma" <[log in to unmask]>
>Encoding: 52 Text
>To: [log in to unmask]
>Cc: [log in to unmask]
>Subject: Re: Solder bridging after wave solder
>Resent-Message-ID: <"dIt133.0.EbD.gozNp"@ipc>
>Resent-From: [log in to unmask]
>X-Mailing-List: <[log in to unmask]> archive/latest/12234
>X-Loop: [log in to unmask]
>Resent-Sender: [log in to unmask]
>
>     Hi Elizabeth -
>     
>     You might try investigating the compatibility of the soldermask and 
>     the flux chemistry. I have found that the soldermask texture (i.e. 
>     either shiny/smooth or matte/rough) and the specific flux interaction 
>     is very important. The general industry trend is that shiny soldermask 
>     will have more solderballs/bridging than matte soldermasks but I have 
>     found that with certain flux chemistries I can use shiny soldermasks 
>     with no solderball/bridging problems. Good Luck.
>     
>     
>     Dave Hillman
>     Rockwell Collins
>     [log in to unmask]
>
>
>______________________________ Reply Separator
_________________________________
>Subject: Solder bridging after wave solder
>Author:  [log in to unmask] at ccmgw1
>Date:    4/23/97 7:19 PM
>
>
>Dear Technet,
>I have a customer who is reporting bridging on the solder side of the board 
>after wave soldering.  I have seen the boards, and they look quite messy, 
>with solder sticking to the mask as well as between component leads and 
>pads.  The mask itself is adhering nicely.  The mask is PC501 from Haven, 
>with C101 hardener.  This was recently discontinued by MacDermid and picked 
>up by Haven.  The flux is no clean, ENFLUX NCF-8660, and is under pressure 
>with nitrogen.  The wave itself is at 500 degrees F, with preheats set to 
>get the board to 210 to 220 degrees F when it hits the wave.  The same 
>design board with LPI ran fine, so I do not suspect a problem in another 
>area of the process.
>     
>No other customers are reporting this problem, and I am at a loss as to 
>where to investigate further. The customer is not happy, and wants a 
>resolution today!  If anyone has any insights, please let me know.
>     
>Thanks,
>Elizabeth Falk
>Process Engineer, Beaverbrook Circuits
>     
>*************************************************************************** 
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
>*************************************************************************** 
>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
>* with <subject: subscribe/unsubscribe> and no text in the body.          * 
>*************************************************************************** 
>* If you are having a problem with the IPC TechNet forum please contact   * 
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
>***************************************************************************
>     
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>***************************************************************************
>
>
>
--------------------------------------------------
Annie Laberge
--------------------------------------------------
Matrox Electronic Systems (MES)

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2