some years ago (in the 93 to be precice) i've evaluated a no-clean fluxer
(RF 32-DM, alphagrillo) with passable ionic contamination and resulting in a
excellent adhereance of the subsequent applied conformal coating (a PUR
based Peters-type) over 4 different solder resist types.
This result was found for no-cleaned as well as cleaned with 4 different
solvents resp. saponifiers (at this evaluation we have compared 11 different
fluxers)
grüsse aus Zürich-Nord
Bernhard
> -----Ursprüngliche Nachricht-----
> Von: Mike Lang [SMTP:[log in to unmask]]
> Gesendet am: Donnerstag, 17. August 2000 21:40
> Betreff: CONFORMAL COAT OVER NO CLEAN
>
>
> Gents,
>
> I have a product which I wave solder with no clean flux. I have a special
> one time application where it is being suggested that we conformal coat a
> series of PCB's. The PCB's will be in a mounted in a NEMA type 4X
> enclosure which will be located outside.
>
> I have only known conformal coating to be applied to PCBs which were
> cleaned, and which passed ionic contamination testing.
>
> We do not clean nor do we have the ability to clean. We do pass the
> standard litany of tests (known because we did extensive testing when
> cutting over to no clean).
>
> What am I in for here?
>
>
>
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|