TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wbVMH-000BjMC; Tue, 10 Jun 97 13:09 CDT
Encoding:
43 Text
Old-Return-Path:
Date:
Tue, 10 Jun 97 13:12:01 cst
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13277
From [log in to unmask] Tue Jun 17 10:
37:29 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"VIxzy3.0.lVI.OXPdp"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
>From willli Tue Jun 10 13:
10:07 1997
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (55 lines)
     Hi TechNet -
     
     Try dropping an email to Doug Pauls at Contamination Studies Labs 
     ([log in to unmask]) - he maybe able to help you.
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Assy: white residues
Author:  [log in to unmask] at ccmgw1
Date:    6/5/97 11:13 AM


     
Hello,
     
We have some white residues in some through hole male connectors after the 
wave soldering operation. They're located "on the floor" of the connectors, 
around the pins. These residues have a granular form, somewhat like salt. It 
could be OA flux residues but I'm not sure.
     
I tried to send the boards through the wave machine without using the solder 
bath to get the fluxing and heating action and it doesn't work. Pressure 
water cleaning alone doesn't work either. The residues can be mechanically 
removed but it is quite time consuming and not practical.
     
Any idea on how to prevent/remove it ?
     
Thank you.
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2