Unless you have a clue as to what the contaminant is, it may be quite difficult to
actually measure. A practical detection test would be to coat a sample with a lacquer
using a similar resin base to your adhesive and put it in the steam zone of a pressure
cooker for a few hours. If it vesicates, then you have problems. This way, you can
determine which cleaning method removes the contaminant best. If it is a silicone, you
may find there is little which will be sure of 100% removal.
Brian
"marvin v. picardal" wrote:
> Dear Techneters,
>
> I would like to ask some help as to how to detect contamination
> on metal surface and how to detect what kind of contamination that is.
> The said contamination results to poor adhesion between the glue and
> the metal surface.
>
> Thank you very much. Hope you would take time in helping me out with this.
>
> Marvin
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|