TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
phil bavaro <[log in to unmask]>
Date:
Tue, 22 Feb 2000 21:48:23 -0800
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, phil bavaro <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
Does anyone have a good procedure that I could use to apply dye penetrant
to detect cracks in BGA connections?
Or is this type of testing better off left to the experts at a test lab?

We have some test vehicle circuit cards which are failing electrically test
after subjecting them to thermal shock cycles.

The failures are no longer intermittent at room temperature so I don't
expect to find just microcracking, but I don't want to just rip the
component off either.

These are test vehicles on which we hoped to determine how close to a BGA
that hardware (screws) attaching the circuit card to a chassis can be
placed without deleterious effects as well as to determine the effect of a
compressive thermal transfer sheet material on the BGA connections.

Any information would be appreciated.

Phil Bavaro

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2