TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Ken Patel <[log in to unmask]>
Date:
Wed, 13 Oct 1999 16:13:18 -0700
Content-Type:
text/plain; charset="us-ascii"
X-To:
Rick Thompson <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ken Patel <[log in to unmask]>
Parts/Attachments:
text/plain (111 lines)
Rick,
Is it irrespective of prior baking and vacuum sealing that part must be
baked before placement/reflow?

We have seen a recent problem on our board with CSP that unbaked parts
created solder bridges. The very next kit we ran, we baked parts and found
no defect. Meaning what you are saying is true.

re,
ken patel

At 01:44 PM 10/8/1999 -0700, Rick Thompson wrote:
>Richard,
>
>Check out the Jedec J-STD-033 ( http://www.jedec.org ). Level 6 parts are
>listed as requiring a mandatory bake prior to reflow. Moisture barrier bags
>and humidity indicator cards are listed as optional. My interpretation of
>this is that while you may want to seal the parts for other reasons, such as
>maintaining lead solderability, it's not required for moisture sensitivity
>reasons alone.
>
>Regards,
>
>
>Rick Thompson
>Ventura Electronics Assembly
>2665A Park Center Dr.
>Simi Valley, CA 93065
>
>+1 (805) 584-9858 voice
>+1 (805) 584-1529 fax
>[log in to unmask]
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]]On Behalf Of <Richard Tilbrook>
>Sent: Friday, October 08, 1999 12:37 AM
>To: [log in to unmask]
>Subject: [TN] level 6 moisture sensitive smt components
>
>
>Hi,
>
>I am enquiring into the acceptable conditions [ie. temp. and Relative
>Humidity] for long term storage [ie. 8 to 10 months] of level 6 moisture
>sensitive smt components.
>
>I am aware that moisture sensitive components of levels 2 through 5 require
>an RH of less than or equal to 20% RH for long term storage, but does this
>apply to levels 5a and 6, or is a lower RH necessary? I ask as I have no
>level 5a information to check on, and level 6 information is individual to
>the component.
>
>Thankyou for taking the time to read this,
>
>Regards,
>
>Richard Tilbrook,
>Junior Engineer,
>British Aerospace.
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
>
______________________________________________________
Ken Patel                       Phone:  (408) 490-6804
1708 McCarthy Blvd.             Fax:    (408) 490-6859
Milpitas, CA 95035              Beeper: (888) 769-1808

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2