TECHNET Archives

February 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Wed, 16 Feb 2000 11:04:23 +1100
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (71 lines)
Hi Ed,

Underfill 1&2 after reflow would be my choice .
For seep in's >start< with dispensing folks
(still love camelots/speedo's/whatevernow) ;
as they did much more validations of various polymers we could ever do .

'm sure Alan reads this somewhere in Net abyss octopusy cave ;
just appear vulnerable and let him/'em pounce (do the work for you) .

if you have different gear , follow same recipe, in their interest to appear
solid .
Did good job for me (each possesses a discretely distributed "reco" list,
changes with evo)
Trust 'em (with caution)

pk

-----Original Message-----
From: Ed Hare [mailto:[log in to unmask]]
Sent: Wednesday, 16 February 2000 2:42
To: [log in to unmask]
Subject: [TN] Dbl-side BGA Assy


Hi all,

I have a couple questions regarding dbl-sided BGA assembly and underfill
...

1)  Would the process typically be ...
Reflow Side 1 > Underfill Side 1 > Reflow Side 2 > Underfill Side 2
or
Reflow Side 1 > Reflow Side 2 > Underfill Sides 1 & 2?

2)  Do any of you have a recommendation for underfill material(s) that
you use and work well?

Best regards,
Ed Hare
VM SEM Lab, Inc.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2