TECHNET Archives

November 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Fri, 21 Nov 2003 15:32:34 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<OFBB1A15C6.DA201ED3-ONC1256DE5.0039AA3F-C1256DE5.003CECD1@LocalDomain>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (87 lines)
Tin has a great affinity for gold and if you can't use a tin free solder
(a similar MP indium/lead for example) then you are somewhat.... "stuck"
is the polite word. There are no alloying additions which will slow down
Au take up or "pre-saturate" the solder.

If you have to use a tin based solder then the only way to reduce the
amount of gold leaching is to reduce the amount of gold. (thinner
coating , mask areas, etc). You can slow down the rate of dissolution by
reducing the temperature, but this probably wouldn't be significant in
practice.
Sometimes if Au embrittlement is a concern you can wash the gold off in
(tin based) solder and then ideally re-coat (with tin based solder), but
that's rather expensive in time even if possible, and gives a two time
heat hit before assembly even begins.

Finally and perhaps counter intuitively you could consider a higher tin
content solder. If that were possible it would reduce the effective
concentration of the gold with respect to the tin.

Regards

Mike Fenner

Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hugues Colicis
Sent: Friday, November 21, 2003 11:02 AM
To: [log in to unmask]
Subject: [TN] Gold diffusion into a tin based solder.


Hi all,

I'm looking for a way to reduce the gold diffusion into a tin based
solder (except the use of the expensive Au/Sn solder). Is there alloys
that have this effect? Or can it be reached by the contamination of gold
by some metals (like Pt, Pd, Cd,...)?

I know the gold embrittlement phenomenon and this is not an issue here
but well the "consumption of gold by the solder".

Thank you for your help,

Hughes Colicis
Process Engineer
Vishay - BCcomponent

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2