Bright Electroplated Tin (OMG product) used as an excellent etch resist by several PCB shops. You can contact OMG Minnesota for more information.
Regards
 
Aleks Lozinsky
Technical Sales Representative
Technic Canada Inc.
Office: 905-940-4020
Cell:  416-450-1093
E-mail: [log in to unmask]

-----Original Message-----
From: Cedric ORAIN <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date:         Wed, 30 Jun 2010 19:03:53 
To: <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>,
        Cedric ORAIN <[log in to unmask]>
Subject: [TN] Bright tin

Hello all,

I've been proposed Bright Tin as PCB finishing. It is the first time I've
heard about this plating for PCB. 

Is someone is familiar with this process and could expose drawbacks and
benefit? 

Do you confirm that it is an electroplating process? Do I need to specify a
Nickel barrier or something lie that underneath the tin layer? Is the
thickness of tin is critical and has to be monitored carefully? 

I'm also concerned about tin whiskers with bright tin as it as been banned
from the plating of connectors and components due to its propensity to the
growth of whiskers.

Ok, it's a lot of questions!  I just want to be advised on what is important
to know about that subject.

Thanks in adavance for your bright advice.

Cedric ORAIN





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2