Is the temperature variation only on the high side, or is the range actually
520-680 for a 600 degree tip? Also, how is the temperature measured? It is
my understanding that unless a thermocouple is embedded into the tip,
temperature measurements are not very accurate due to air currents, the
quality of the contact between tip and measurement device, etc.
=========================
Bob Barr
Manufacturing Engineering
Formation, Inc.
Voice: 856-234-5020 x3035
Fax: 856-234-6679
=========================
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Thursday, June 20, 2002 1:57 PM
To: [log in to unmask]
Subject: Re: [TN] Metcal SP200 soldering Iron
In a message dated 6/18/2002 4:06:29 PM US Eastern Standard Time,
[log in to unmask] writes:
<< My only gripe with the Metcals is the cost of tips vs. their
life expectancy. >>
I also have a problem with their temp control. They have quite a wide range
for each cartridge. Five tips of identical part number may range as much as
80 degrees, and Metcal will acknowledge that as within their acceptance
criteria. So when you plug in a "600 degree" tip, you might get anything
between 600-680 degrees, with no way of telling one from the next.
Jon Moore
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|