I have done this before, regarding the hot air reflow method. I will not
lie...it's difficult and requires very strict concentration. I would lay a small
bead of paste out of a dispenser along the lead array on all sides and carefully
lay the part on pads, sometimes tacking one lead on each corner with
conventional iron and then using the hot air to flow the rest of the leads. This
will cause bridging, but that can taken care of after the fact. The most
critical part of this was to use very fluid movements and reflow all of the
leads at the same time and evenly, going around all of the leads in a circular
motion. If this is not done right, pads can be damaged easily. Try a scrap board
and dummy part first, if possible.
Jason Gregory
Production Supervisor
LaBarge Inc.
(918)459-2367
[log in to unmask]
Ron Olinyk <[log in to unmask]> on 11/27/2002 03:48:30 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond to
Ron Olinyk <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Jason Gregory/LABARGE)
Subject: [TN] Hand soldering fine pitch SMT
Can anyone recommend good soldering technique for
hand assembly of 20mil pitch devices and 0603, 0402
SMT chips? We are looking at doing some protoype
assembly on some fairly dense (and small) pcbs. We
were thinking of using solderpaste and one of those
portable solder pens with a hot air tip ie. Weller
Portasol. Has anyone had success using this
technique?
Thanks
Ron.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|