TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], Ingemar Hernefjord <[log in to unmask]>
Date:
Thu, 8 Jul 2010 06:49:05 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Drew meyer <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="windows-1252"
Content-Transfer-Encoding:
quoted-printable
From:
Drew meyer <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Inge,

There might be some confusion on the stucco form depending on ones 
location.  

Here in the states such work was done on ceilings into the very early 1900's.  
Not sure if it was applied much after that.  The decorative parts were formed 
up with plaster, sometimes with burlap added for reinforcement on long pieces, 
then taken to the building site and installed.  The only applications now are 
restorations of old buildings where the owners want to go back to the original 
ceiling.  At a minimum you have to have one of each part available to make 
the molds or shaping tools.

In general we use the term stucco for a mortar/cement like mixture spread 
over metal mesh on the exterior of a building.

Sounds like your ceilings are a feast for the eyes.  As a rule ours are quite 
plain now.

Drew

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2