TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sun, 3 Aug 2003 00:54:42 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
In a message dated 08/02/2003 0:50:34, [log in to unmask] writes:
>By now I have seen quite a bit of ATC presentations for Lead Free and I am
>a bit surprised that this is the first time I have read about a soak or
>dwell time at each temperature extreme. Most have reported that they just
>go up and then back down in temperature. 30minutes up and 30 minutes down,
>thus 24 cycles a day across the range they have selected seems quite common.
>Any comments??
>Have you also seen this type ATC procedure?

Hi Dave,
Yes, unfortunately I have seen them--and it's a pity. These data are worse
than useless--they are misleading. But that comes from people doing things
without understanding them, and from people being pushed to produce data
fast--nevermind that they are meaningless

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2