Hi Jim,
The attached photo got stripped from your message by the list serve. This
minimizes the opportunity of spreading viruses through the list, which has
shrunk from it's lofty heights of 2000 +/- how many Steve?
You have three choices well two really:
1). Snail mail a copy of the photo to each of us. Preferably in 8 x 10 matte
format along with your other headshots. (Okay, I did a bit of casting work
while at USC. hee hee.)
2). Post the image to your webpage - personal or business.
3). Post the image to an on-line hard drive such as http://www.driveway.com
and then send us the sharing link, for example:
http://www.driveway.com/share?sid=a8f3cb1d.96df8&name=Pictures where
everyone can see the scratches and oily residue on those double treat panels
I mentioned the other day. (No implied endorsement of driveway.com or I'll
have OSI asking me questions.)
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials Engineer (Process & Manufacturing)
Warner Robins Air Logistics Center
Avionics Production Division
Precision Attack/ Radar/Manufacturing Branch
Engineering Section
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (478) 926 - 1970 Fax: (478) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
-----Original Message-----
From: James Moffitt [mailto:[log in to unmask]]
Sent: Tuesday, October 03, 2000 7:29 PM
To: [log in to unmask]
Subject: [TN] Photo
Hi Carl:
- Scrounging around the harddrive netted a photo of the condition I
discussed. In the attached photo the dark area just below the meniscus of
the outer heel fillet (J-Lead device) is a group of solder balls that are
entrapped by the partially reflowed solder paste. Needless to say, this
condition does nothing to enhance the reliability of the solder connections.
Will provide additional photos when I return the office on Friday. Hope you
don't find something like this in your microsectional analysis.
Regards, Jim Moffitt, Technical Director, Electronics Training Advantage,
Indianapolis, IN
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|