OK on the Vanillin/Palladium. Just wondering how much acid copper you are
getting in the center of the holes? If the MacDermid carbon black direct
metallization is not compatible with the acid copper, we get less in the
center.
However, you need to solve the drilling/laminate problem, because even if
copper does plate around the glass fibers, the boards seem to absorb water in
storage and blow hole at assembly. Then, your customer will complain
whenever assembling parts - one to twelve months from now.
One final tip - cross section some holes 45 degress from the weave. Cross
sections usually are with the weave - just the way we drill holes in a
straight line and cross section to get the most holes. 45 degress cross
sections will reaveal the most resin "chunking" and the most glass bundles
torn. Good luck
Denny Fritz
MacDermid
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|