TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Jones, Heidi N (NM75)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 24 Apr 1998 15:54:39 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (65 lines)
Hi Werner,

We use both, depending on the test specification, so I am curious, how do
the damage and/or failure mechanisms differ between thermal cycling and
temperature cycling?

Heidi Jones
Senior Manufacturing Engineer
Honeywell, Defense Avionics Systems
9201 San Mateo NE
Albuquerque, NM 87113-2227
(505) 828-5806
FAX (505) 828-5500
email: [log in to unmask]


----------
From:  Engelmaier[SMTP:[log in to unmask]]
Sent:  Friday, April 24, 1998 3:42 PM
To:  [log in to unmask]
Subject:  Re: [TN] high temperature solders

Hi Ed,
Thermal shock is NOT an accelerated test for loading due to thermal
cyling.
The damage mechanism is different then thermal cycling and therefore
passing a
thermal shock test does not assure 10 years of life in thermal cycling.
Thermal shock can be used for ESS and for HAST testing to increase general
robustness.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2