This could also be an issue of inventory/material availability.  The
fabricator may not have 1 oz copper in stock.

Another issue is the use of electrolytic nickel/gold.  There are galvanic
etching problems with the combination of Cu/Ni/Au as well as overhang/leaf
of the gold plating.  The more you have to etch through the more this can
become a problem.  0.5 oz copper in place of 1 oz makes sense in this
application.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cal Driscoll
Sent: Wednesday, July 28, 2004 5:20 AM
To: [log in to unmask]
Subject: [TN] 1oz Copper vs. .5 oz Copper

Hi All-

One of our PCB designers came to us with a recommendation from our Bare
Board fab house-
We typically use 1 oz copper and the fab house is asking us to use .5 oz
copper and build it up to 1 oz.

Since I am not a designer, so I would like some input from TechNet on this
type of practice.

Facts:
99% of our boards are used in Telecommunications products
Most of our boards have QFP's in the 12 mil range
Typically most of our boards have Gold pads/finish


Thanks,
cal

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2