TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Stephen Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stephen Gregory <[log in to unmask]>
Date:
Mon, 5 Dec 2005 08:49:02 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
Good Morning Everyone!

I got Wee Mei's picture up...go to:

http://stevezeva.homestead.com/files/Soldermask_Defect.JPG

I've seen this before, but I can't explain it either.

Kind Regards,

-Steve Gregory-

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wee Mei
Sent: Sunday, December 04, 2005 6:58 PM
To: [log in to unmask]
Subject: [TN] What is this solder mask defect?

Steve,

Hello,

The suspect is completely flat and smooth to touch. An interesting
observation is that though it appear at the same location for all the
10pcs
of board, the size of the image tend to get smaller and smaller if the
boards are arranged starting with the largest image. It can't be soda
strawing as it is not on trace. It can't be pink ring as it is not
around
hole. What can it be? What is the likely cause?

Will ask Steve to put it up. Kindly take a look. Your opinion is greatly
appreciated.

Regards,
Wee Mei

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2