You may want to specify a minimum of 150 microinches of electroless nickel
compared to the standard of 100. It is just a matter of extending the dwell
time in the nickel by about 10-15 minutes. The cost is minimal unless you
are talking about extremely large volumes.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dwight Mattix
Sent: Wednesday, December 12, 2007 3:02 PM
To: [log in to unmask]
Subject: Re: [TN] Gold Finger plating question.
Yep. ENIG has worked fine for us in some lower cycle insertion apps. YMMV
depending on specifics of your app and the connector style used.
At 11:07 AM 12/12/2007, you wrote:
>I have a small panelized SMT SIM module with gold fingers that I was
>going to use ENIG for the entire board including the gold fingers. I
>was not going to use the standard gold tip process. This board only
>requires one or two insertions. Once it is installed most likely it
>will never be removed from the socket. I've done this on a similar
>board with no issues but wanted some feedback from my fellow
>Techneter's.
>
>
>
>Thanks in advance,
>
>
>
>Scott
>
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|