TECHNET Archives

September 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Sat, 11 Sep 2010 14:54:24 -0400
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (67 lines)
Hi,

 

 If I had a sensitive scale I would try this myself, I was wondering if
anyone out there could try this simple experiment.

 

Goal: Get an idea of how much water is left on a board after rinse and blow
off.

 

 If someone could take a board with parts on one side, rinse in water, then
make these measurements.

 

1.    Weigh a PCB with parts on one side. Record size and weight.



2.    Rinse board under water spray.



3.    Shake off free water then measure weight of board.



4.    Blow of water with air gun then measure weight.



5.    Oven dry then weigh.



 I realize there is a lot of variations in PCBs and this is controlled test
by any means. But I am curious to get a first order approximation.

I would love to see the numbers.

 

Thanks,

Bob Kondner



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2