Hi Jeff,
For our eutectic PBGA's, we only flux (no clean). Have only done about 50
or so over the past year with very good (97% yield) results.
Have not seen any studies or papers. Just worked closely with our CM to
create the profile for each type of BGA. We use Air-Vac.
Kerry
-----Original Message-----
From: Jeff Ferry [mailto:[log in to unmask]]
Sent: Thursday, January 31, 2002 11:54 AM
To: [log in to unmask]
Subject: [TN] BGA Rework Using Paste vs. No Paste
Fellow TechNetters,
We nearly always apply solder paste to the circuit board when we replace
BGA components during rework. Yet, after speaking with a handfull of BGA
equipment companies at APEX, seems like they all recommend using flux only
vs. paste, unless the circuit board is used in a high rel application.
What do ya'all do/recommend for BAG rework? Can you point me to any
studies/reports on the subject?
Thanks,
Jeff Ferry
CEO
Circuit Technology Center, Inc.
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|