Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Sat, 22 Jan 2005 09:58:55 +0200
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gabriela Bogdan <[log in to unmask]>
Content-type:
text/plain; charset=iso-8859-1
Subject:
From:
Gabriela Bogdan <[log in to unmask]>
Content-transfer-encoding:
QUOTED-PRINTABLE
Parts/Attachments:
text/plain (53 lines)
http://www.derweg.org/personen/werke/glocke.html
Von der Stirne heiß
Rinnen muß der Schweiß,
Soll das Werk den Meister loben,
Doch der Segen kommt von oben.

----- Original Message ----- 
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, January 22, 2005 2:17 AM
Subject: Re: [TN] Lead-free Wave Solder Pot Impurity Levels


> Hi Gaby,
> No, reliability tests cannot remain the same, because they do not mean the
> same. Having said this,I must add that we do not know enough to say what
they
> mean.
>
> Regards,
> Werner Engelmaier
> Engelmaier Associates, L.C.
> Electronic Packaging, Interconnection and Reliability Consulting
> 7 Jasmine Run
> Ormond Beach, FL 32174 USA
> Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
> E-mail: [log in to unmask], Website: www.engelmaier.com
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2