Guenter,
It may be just an oxide spot on the copper.  The solder mask will not adhere well to the copper oxide and can even get a small gas bubble between.  It may not be a big problem, if the oxide is not an
acidic contaminant then the trace will probably not be a reliability problem.  It could also be an organic contaminant, also not a problem if it has not already caused a failure.

Look at it under high power (like 200X) and if the copper is full height forget about the spot.

Chuck Brummer


Guenter Grossmann wrote:

> Hi all
>
> I have a case here where I am not sure what I see.
> - There are dark spots visible below the solder mask on the surface of the traces on a PCB. I attached 2 Pictures in JPEG that show a view onto the surface of the traces with 10x and 40x magnification.
> - In microsections we see clearly a cavity between the traces and the soldermask.
> - EDX is hopeless, since the dark layer is so thin that the background covers all but the copper peak.
>
> Before I start to work with TOF SIMS, Spectroscopy and other expensive analysis methods I'd like to ask whether one of you knows what the dark spots are.
>
> Thanks in advance. Have a great day.
>
> Guenter
>
> Guenter Grossmann
> Swiss Federal Institute for Materials Testing and Research EMPA
> Centre for Reliability
> 8600 Duebendorf
> Switzerland
>
> Phone: xx41 1 823 4279
> Fax :      xx41 1823 4054
> mail:     [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2