     Neil,

     To get the most of your request, I recommend you go to the source(s).
     Few suppliers, unless there are any old MIL companies online carry
     11.5oz of copper clad.

     Try the following companies, the numbers may have changed, but at
     least you have the company name for starters.

     1. Copper Clad Multilayer
        714-237-1388

     2. Nelco Products
        714-879-4293

     3. NVF
        610-444-2800

     4. Polyclad Laminates
        603-934-5642

     5. Electroply
        310-322-5647

     6. Century Laminators
        714-828-2071

     7. Arlon
        909-989-7053

     8. Allied Signal
        608-784-6070


     John Gulley
     Inet Technologies Inc
     A Smarter Vision


______________________________ Reply Separator _________________________________
Subject: [TN] 11,5 oz Double Sided FR4
Author:  Neil Atkinson <[log in to unmask]> at Internet
Date:    11/4/98 7:43 AM


Hi all,

This is the second time I've asked this question and last time I
received a good response with a few good contacts but I have still been
unable to find a source of 11.5 oz double sided FR4.  I have a contact
for CEM1 and this may be OK but I would still be interested if anyone
out there could supply FR4 to this spec.

While I'm on the subject what are the main differences in the properties
of FR4 and CEM1?

Thanks in anticipation of everyone's usual excellent response.


Neil Atkinson

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2