Graham
The copper will let go off the laminate long before intermetalic shear .
That is with properly designed pads , components, & process ( IPC strds,
say )
>----------
>From: COLLINS, GRAHAM[SMTP:[log in to unmask]]
>Sent: Wednesday, 4 February 1998 6:23
>To: [log in to unmask]
>Subject: solder shear strength
>
>Technetters - I know someone has this information at their fingertips. I'm
>in an argument with someone about a socket, and I have to prove that a
>gorilla would have to stand on the part to shear the solder joints holding
>the socket on the board (it's a PGA component). Can someone tell me the
>shear strength of solder? I'm going to construct a very crude mathematical
>model.
>
>As always, Thanks!
>
>regards,
>
>Graham Collins
>Process Engineer,
>Litton Systems Canada
>(902) 873-2000 ext 215
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|