I am looking for a solution to break up ceramic substrates.  The 
conventional cutting/routing tools may not work well due to possibility 
of micro-cracks.  I have heard that some vendor has developed some kind 
of rollers (air inflated) that naturally breaks the substrates when 
passing the substrates through.   

Will appreciate any advice.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2