TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 23 Sep 2005 15:52:52 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (35 lines)
Hi Ioan,
Your heat/freeze=it works, ambient temperature=fail points to some
intermittent opens
2 possibilities: (1) fractures SJs, (2) fractures PTV barrels.
(2) is less likely, because it typically results in freeze=it works,
heat/ambient temperature=fail;
(1) is most likely given your descriptions. Have you tried press-down on
BGA=it works? Your heat/freeze=it works is indicative of some BGA/PCB warpage.
Possible causes: excessive BGA warpage due to thermlly unsymmetric design;
thermal shock cracking due to rapid cooling after reflow.
But, until you know what the problem is--let alone what the root cause(s)
is(are), you cannot even think of a fix.



Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2