TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Date:
Tue, 12 Aug 1997 15:50:10 +0000
Reply-To:
Content-Transfer-Encoding:
7BIT
Content-Type:
text/plain; charset=US-ASCII
Subject:
From:
Wesley Samples <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Organization:
EFW, Inc.
Comments:
Authenticated sender is <samples@[138.32.59.15]>
Parts/Attachments:
text/plain (22 lines)
Hello technet

Wondering if anyone out there that is using Armakleen is seeing paper
like fibers clogging there recirculating pump filter in the wash bath.

We are experiencing this problem and have not identified a source to
date.

We have already done the common sense stuff;
Drain & Clean
Descaling
Limit material going in ie..paper products

Any feedback would be appreciated

And as always,
thanks in advance

Wesley Samples
[log in to unmask]