Use a 700 degree F tip, stay off the pad and raise the tip to touch
the lead of the component only, with the solder tip, instead of the pad to
avoid burning the board or lifting pads because it may be necessary to keep
touching the solder connection up to 9 seconds. Some boards are delicate and
some are not, it all depends.
In one special case, it was necessary to heat up the board to 275
deg F by having the board up side down on a hot plate while it was being
soldered to get the minimum of 60 percent penetration. Good luck.
Regards,
Ramon
> -----Original Message-----
> From: Don_well [SMTP:[log in to unmask]]
> Sent: Monday, June 16, 2003 2:45 AM
> To: [log in to unmask]
> Subject: [TN] High heat sink board hand soldering
>
> Hi all
>
> As we know hand soldering PTH component is difficult on a tens-layer
> boards because of high heat sink.The solder volume filling level is always
> less than 50%. Could you please give me any ideas to settle this
> problems.Below is only for referrence.
>
> 1 Preheat the board about 100 degrees before rework.
>
> 2 Design a enlarged pad before manufacture.
>
> 3 >=25% solder level is acceptable.
>
> Thanks for your advice.
>
> B.Regards
>
> Don
>
> Huawei Tech Ltd
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|