     LaVern,
     
     I have used .007 W/in-C for the FR4 material (not including copper 
     layers) with good success.  
     
     Frank Hinojos
     Watkins-Johnson Co.


______________________________ Reply Separator _________________________________
Subject: DES:FR-4 Thermal Conductivity
Author:  [log in to unmask] at INTERNET
Date:    7/22/97 2:05 PM


     
     
     
     
Can anyone tell me what the "Thermal Conductivity" is for FR-4 material? 
Where can I find this info?  and what FR-4 materials, if any, are better 
suited to transfer heat?
     
Thank you, in advance, for your responses!
     
LaVern Mullet
Thomas & Betts
[log in to unmask]
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2