TECHNET Archives

October 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Tue, 13 Oct 1998 12:24:55 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (28 lines)
Greg -
I don't see what the advantages of aluminum tape would be over Kapton tape for
attaching TCs.  Neither provides firm (non-lifting) attachment as evidenced by
the noice one sees when the profile is plotted out.  You really do not know
what you are "probing" but it likely is not a good representation of the
solder joint.
High temp solder is best,  conductive epoxy a good substitute.  If you
absolutely cannot sacrifice a board to the "profile gods", I suggest the use
of the TempProbes from Saunders.  Not as good as the solder or epoxy, but a
close second and far better than using tape.

Phil Zarrow
ITM, Inc.
Durham, NH
www.ITM-SMT.com

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2