All fluxes for In soldering should be halide free as In is attacked by
halides.

Gel or tack fluxes with the same fluxing abilities as their solder paste
analogues are readily available. 

Getting fluxes to "activate" at reduced process temps is not so much of an
issue, but generating full no clean properties might be, discuss with
supplier.

 

Best Wishes

 

 

 

Mike

  _____  

From: Larry Dzaugis [mailto:[log in to unmask]] 
Sent: Saturday, March 30, 2013 8:42 PM
To: [log in to unmask]
Subject: Re: [TN] solder which does ot scavenge gold

 

Be sure to use a compatible flux, one that activates at a lower temperature.

An Indium alloy solder paste will have the correct flux.

It is when preforms or solder wire are used. 

Typical paste activates around the melting point of 100% Indium.

Learned this from an inherited hand solder and vapor phase assembly.

 



 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2