TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Jorge Engenharia <[log in to unmask]>
Date:
Fri, 28 Apr 2000 09:39:05 -0300
MIME-Version:
1.0
X-To:
"Jason Larson, CET" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jorge Engenharia <[log in to unmask]>
Parts/Attachments:
text/plain (54 lines)
 Jason;

  This could happens in all phases but generally you can check the following
:

  Check Z spam seeing if the terminal is at the center of the hole
  The board must be flat
  Reduce the clinch angle ( adjust cutter/former screw )
  Increase Depth Stop

I hope this help
Jorge Dourado de Santana
Maintenance / Process Engr
Microtec - Brazil


> -----Original Message-----
> From: Jason Larson, CET [SMTP:[log in to unmask]]
> Sent: 27 de Abril de 2000 20:32
> To:   [log in to unmask]
> Subject:      [TN] auto insertion
>
> Hi Technet,
>
> This question is for those that are experts in auto insertion,
>
> At what phase of insertion (depth stop setting, lead shear, clinch, Z
> span)
> are you most likely to break a fragile component such as a glass pack
> diode
> or ceramic axial cap.
>
> We use a Universal VCD
>
> Thanks in advance,
>
> Jason
>
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2